Our primary target will be to provide our clients a serious and responsible small business relationship, supplying personalized attention to all of them for Steel Pipe Kg Per Meter, Tube, Astm A 335 P11 Alloy Pipe, We have been wanting forwards to creating long-term company interactions with around the world shoppers.
Erw Tube Sch 120 - Seamless Medium carbon steel boiler and Superheat tubes ASTM A210 standard – Sanonpipe Detail:

Overview

Application

It is mainly used to make high-quality seamless carbon steel, for boiler pipes, super heat pipes

for bolier industry , heat changer pipe etc. With difference sizes and thickness

Main Grade

Grade of high-quality carbon boiler steel: GrA, GrC

Chemical Component

Element Grade A Grade C
C ≤0.27 ≤0.35
Mn ≤0.93 0.29-1.06
P ≤0.035 ≤0.035
S ≤0.035 ≤0.035
Si ≥ 0.1 ≥ 0.1

A For each reduction of 0.01 % below the specified carbon maximum, an increase of 0.06 % manganese above the specified maximum will be permitted up to a maximum of 1.35 %.

Mechanical Property

Grade A Grade C
Tensile Strength ≥ 415 ≥ 485
Yield Strength ≥ 255 ≥ 275
  Elongation rate ≥ 30 ≥ 30

Test Requirement

Hydraustatic Test:

The Steel Pipe Should Be Tested Hydraulically One By One. The Maximum Test Pressure Is 20 MPa. Under The Test Pressure, The Stabilization Time Should Be Not Less Than 10 S, And The Steel Pipe Should Not Leak.

After The User Agrees, The Hydraulic Test Can Be Replaced By Eddy Current Testing Or Magnetic Flux Leakage Testing.

Flattening Test:

Tubes With An Outer Diameter Greater Than 22 Mm Shall Be Subjected To A Flattening Test. No Visible Delamination, White Spots, Or Impurities Should Occur During The Entire Experiment.

Flaring Test:

According To The Requirements Of The Purchaser And Stated In The Contract, The Steel Pipe With Outer Diameter ≤76mm And Wall Thickness ≤8mm Can Be Done Flaring Test . The Experiment Was Performed At Room Temperature With A Taper Of 60 °. After The Flaring, The Flaring Rate Of The Outer Diameter Should Meet The Requirements Of The Following Table, And The Test Material Must Not Show Cracks Or Rips

Hardness Test:

Brinell or Rockwell hardness tests shall be made on specimens from two tubes from each lot

Product Detail

Boiler Tube


1


GB/T5310-2017

A106 Boiler Pipe


ASME SA-106/SA-106M-2015


carbon steel pipe


ASTMA210(A210M)-2012


eamless steel tubes for normal structure


ASME SA-213/SA-213M


boiler pipe IBR


ASTM A335/A335M-2018


Product detail pictures:

Erw Tube Sch 120 - Seamless Medium carbon steel boiler and Superheat tubes ASTM A210 standard – Sanonpipe detail pictures

Erw Tube Sch 120 - Seamless Medium carbon steel boiler and Superheat tubes ASTM A210 standard – Sanonpipe detail pictures

Erw Tube Sch 120 - Seamless Medium carbon steel boiler and Superheat tubes ASTM A210 standard – Sanonpipe detail pictures


Related Product Guide:

Our business sticks for the basic principle of Quality could be the life with the firm, and track record will be the soul of it for Erw Tube Sch 120 - Seamless Medium carbon steel boiler and Superheat tubes ASTM A210 standard – Sanonpipe , The product will supply to all over the world, such as: United States, Georgia, United States, With excellent solutions, high quality service and sincere attitude of service, we ensure customer satisfaction and help customers create value for mutual benefit and create a win-win situation. Welcome customers all over the world to contact us or visit our company. We'll satisfy you with our qualified service!
  • This company can be well to meet our needs on product quantity and delivery time, so we always choose them when we have procurement requirements.
    5 Stars By Antonia from Iraq - 2017.12.09 14:01
    In China, we have purchased many times, this time is the most successful and most satisfactory, a sincere and realiable Chinese manufacturer!
    5 Stars By Gemma from UK - 2018.02.12 14:52
    Write your message here and send it to us